Difference Between Alumina And Calcined Alumina

Jul 20, 2022

. Alumina

Pure alumina is a white amorphous powder, commonly known as bauxite, with a density of 3.9-4.0g/cm3, a melting point of 2050°C and a boiling point of 2980°C, and is insoluble in water. Can be extracted from bauxite. Bauxite (Al2O3·H2O and Al2O3·3H2O) is the main mineral of aluminum in nature. It is pulverized and impregnated with high-temperature sodium hydroxide solution to obtain sodium aluminate solution; filter to remove the residue, cool the filtrate and add hydroxide Aluminum crystal, after a long time of stirring, the sodium aluminate solution will separate out aluminum hydroxide precipitate; the precipitate is separated and washed, and then calcined at a temperature of 950-1200 ° C to obtain α-type alumina powder, and the mother liquor can be recycled . This method was invented by the Austrian scientist K.J. Bayer in 1888, and it is still the main method of industrial production of alumina today, known as the "Bayer method". In the lattice of α-type alumina, oxygen ions are hexagonally packed, and Al3+ is symmetrically distributed in the octahedral coordination center surrounded by oxygen ions. The lattice energy is very large, so the melting point and boiling point are very high. Alpha alumina is insoluble in water and acid, also known as aluminum oxide in industry, and is the basic raw material for making metal aluminum; it is also used to make various refractory bricks, refractory crucibles, refractory tubes, and high temperature experimental instruments; it can also be used as an abrasive , flame retardants, fillers, etc.;

High-purity alpha alumina is also the raw material for the production of artificial corundum, artificial ruby and sapphire; it is also used to produce the substrate of modern large-scale integrated circuits. γ-type alumina is obtained by dehydration of aluminum hydroxide at a low temperature of 140-150 ° C. It is also called activated alumina and aluminum glue in industry. In its structure, the oxygen ions are close-packed close to the cubic center, and Al3+ is irregularly distributed in the octahedral and tetrahedral voids surrounded by the oxygen ions. γ-type alumina is insoluble in water, but can be dissolved in strong acid or strong alkali solution, and it is completely converted into α-type alumina when heated to 1200 °C. γ-type alumina is a porous material, with an internal surface area of hundreds of square meters per gram, high activity and strong adsorption capacity. Industrial products are usually colorless or slightly pink cylindrical particles with good pressure resistance. It is a commonly used adsorbent, catalyst and catalyst carrier in petroleum refining and petrochemical industry; it is a deacidifying agent for transformer oil and turbine oil in industry, and it is also used for chromatographic analysis; it is a neutral strong desiccant in the laboratory , its drying capacity is no less than that of phosphorus pentoxide, and it can be regenerated and reused after heating for 6-8h below 175 °C. At present, the alumina produced by the Bayer method in the world accounts for more than 90% of the total output. Most of the alumina is used to make metal aluminum, and less than 10% is used for other purposes.